Every heat is sampled. Every sample is archived. Our testing chain covers composition control before melting, during melting and before pouring — plus metallographic verification after solidification. Records are kept by batch number for two years so any casting can be traced back to its heat.
How do we control casting quality?
1. Carbon–silicon analysis — before the furnace
Rapid furnace-front analysis confirms that charge composition meets process requirements, improving both melt quality and batching efficiency.
2. Optical emission spectrometer — two samples per heat
One sample is taken before tapping to confirm each element is within specification; a second is taken before pouring to verify the final composition.
3. Metallographic analysis — after solidification
Every heat is sampled, with element composition and metallography records filed against the batch number. Samples are stored for two years.
| Control point | Method | Frequency | Record |
|---|---|---|---|
| Charge / pre-furnace | Carbon–silicon analyzer | Every heat | Composition log |
| Before tapping & before pouring | Optical emission spectrometer | 2 samples per heat | Element analysis |
| After solidification | Metallographic analyzer | Every heat | Metallography + element ledger |
| Sample retention | Batch-numbered storage | 2 years | Traceable archive |
Dimensional and appearance control
- Patterns are CNC-formed to reduce parting and bonding deviation from the drawing.
- Drying racks are infrared-leveled to avoid distortion during coating and baking.
- Shot blasting and manual dressing remove sand and flashes before final inspection.
“`mermaid
flowchart TB
A[“Charge material”] –> B[“Carbon-silicon check”]
B –> C[“Melting in 2t induction furnace”]
C –> D[“Sample 1: before tapping”]
D –> E[“Sample 2: before pouring”]
E –> F[“Pouring”]
F –> G[“Metallographic analysis”]
G –> H[“Batch ledger + 2-year sample archive”]
“`